Dedicated Software GLUON Series

M.P. (Multipurpose) Test Package

M.P. (Multipurpose) Test Package

Supports Complicated Measurement & Control

This test package supports almost all type of tests that involves complex measurement and control, such as programmed loading using combinations of different waveform and multi-axis control.

Features

  • Security Function
    User registration function protects test condition files and test data.
  • Simple Setup Using Wizards
    Settings can be made without any input omissions thanks to easy-to-understand wizards.
  • Output of Text Data
    Sample data can be converted and output in text data format. This enables proprietary data analysis in third-party spreadsheet software, for example.

Specifications

Part name GLUON M.P. (Multipurpose) Test Package
P/N 346-99912
Applicable tests Programmed load test
Applicable controller 4890 Controller
Recommended operating environment OS: Windows 2000, Windows XP
CPU: Pentium 800 MHz or faster
RAM: 1 GB min.
HDD: 8 GB min. free space
CD-ROM × 1 unit, 100base-T Ethernet

* Appearance and specifications are subject to change without notice.

Fatigue Test Package

Evaluation of Cycle Fatigue

This software applies cycle load to specimens and evaluates cycle fatigue. It supports all testing from low- through to high-cycle fatigue testing.

Features

  • Security Function
    User registration function protects test condition files and test data.
  • Simple Setup Using Wizards
    Settings can be made without any input omissions thanks to easy-to-understand wizards.
  • Output of Text Data
    Sample data can be converted and output in text data format. This enables proprietary data analysis in third-party spreadsheet software, for example.

Specifications

Part name GLUON Fatigue Test Package
P/N 346-99913
Applicable tests Fatigue testing, low-cycle fatigue testing, bending fatigue testing
Applicable controller 4890 Controller
Recommended operating environment OS: Windows 2000, Windows XP
CPU: Pentium 800 MHz or faster
RAM: 1 GB min.
HDD: 8 GB min. free space
CD-ROM × 1 unit, 100base-T Ethernet

* Appearance and specifications are subject to change without notice.

Static Test Package

Evaluation of Static Strength

This package supports all tensile, compression and bending static testing. Two or more control modes (e.g. stress/strain) and load speeds can be selected.

Features

  • Security Function
    User registration function protects test condition files and test data.
  • Simple Setup Using Wizards
    Settings can be made without any input omissions thanks to easy-to-understand wizards.
  • Output of Text Data
    Sample data can be converted and output in text data format. This enables proprietary data analysis in third-party spreadsheet software, for example.

Specifications

Part name GLUON Static Test Package
P/N 346-99914
Applicable tests Static tensile test, static compression test, static bending test
Applicable controller 4890 Controller
Recommended operating environment OS: Windows 2000, Windows XP
CPU: Pentium 800 MHz or faster
RAM: 1 GB min.
HDD: 8 GB min. free space
CD-ROM × 1 unit, 100base-T Ethernet

* Appearance and specifications are subject to change without notice.

Crack Growth Test Package

Evaluation of Relationship between Crack Growth Rate and ΔK Value

Logical operation functions smoothly control the ΔK value to enable the evaluation of crack growth properties. This package can also be used for introducing pre-cracking of specimens in compliance with KIC and JIC fracture toughness standards.

Features

  • Security Function
    User registration function protects test condition files and test data.
  • Simple Setup Using Wizards
    Settings can be made without any input omissions thanks to easy-to-understand wizards.
  • ASTM E647-compliant
  • Output of Text Data
    Sample data can be converted and output in text data format. This enables proprietary data analysis in third-party spreadsheet software, for example.

Specifications

Part name GLUON Crack Growth Test Package
P/N 346-99915
Applicable tests Crack growth test
Applicable standard ASTM E647
Applicable controller 4890 Controller
Recommended operating environment OS: Windows 2000, Windows XP
CPU: Pentium 800 MHz or faster
RAM: 1 GB min.
HDD: 8 GB min. free space
CD-ROM × 1 unit, 100base-T Ethernet

* Appearance and specifications are subject to change without notice.

KIC/COD Test Package

Calculation of KIC/COD Values

This package can conduct tests compliant with standards to calculate the KIC value and judge its validity. It can also evaluate the COD value.

Features

  • Security Function
    User registration function protects test condition files and test data.
  • Simple Setup Using Wizards
    Settings can be made without any input omissions thanks to easy-to-understand wizards.
  • ASTM E399, ISO 12737-compliant
  • Output of Text Data
    Sample data can be converted and output in text data format. This enables proprietary data analysis in third-party spreadsheet software, for example.

Specifications

Part name GLUON KIC/COD Test Package
P/N 346-99916
Applicable tests KIC/COD test
Applicable standard ASTM E399, ISO 12737
Applicable controller 4890 Controller
Recommended operating environment OS: Windows 2000, Windows XP
CPU: Pentium 800 MHz or faster
RAM: 1 GB min.
HDD: 8 GB min. free space
CD-ROM × 1 unit, 100base-T Ethernet

* Appearance and specifications are subject to change without notice.

JIC Test Package

Calculation of JIC Value

This package enables JIC tests that involve difficult procedures to be conducted simply. After the test ends, a J-Δa graph is created, the JIC value is calculated, and judgment as to the validity of its value is made.

Features

  • Security Function
    User registration function protects test condition files and test data.
  • Simple Setup Using Wizards
    Settings can be made without any input omissions thanks to easy-to-understand wizards.
  • ASTM E813*, JIS Z2284-compliant
    * Bending tests and multiple testing are not supported.
  • Output of Text Data
    Sample data can be converted and output in text data format. This enables proprietary data analysis in third-party spreadsheet software, for example.

Specifications

Part Name GLUON JICTest Package
P/N 346-99917
Applicable tests JICtest
Applicable standard ASTM E813*, JIS Z2284
* Bending tests and multiple testing are not supported.
Applicable controller 4890 Controller
Recommended operating environment OS: Windows 2000, Windows XP
CPU: Pentium 800 MHz or faster
RAM: 1 GB min.
HDD: 8 GB min. free space
CD-ROM × 1 unit, 100base-T Ethernet

* Appearance and specifications are subject to change without notice.

Thermal Fatigue Test Package

For Compound Loads of Heat and Strain

This package provides the specimen with a load such as trapezoidal wave, and records the test force (stress) - displacement (elongation, strain) curve and temperature signals for a specified repeat count. It provides a temperature pattern synchronized with the load and corrects for thermal expansion to enable mechanical strain control and constant constraint rate control. Hysteresis energy and plastic strain can also be calculated from acquired data.

Features

  • Up to ten waveforms comprising multiple steps can be repeated as the load and temperature setting screen loads and temperature signals.
  • Thermal expansion data can be recorded for up to 50 thermal expansion correction data so that mechanical strain control and constant constraint rate control testing can be performing with thermal expansion factored in.

Specifications

Part name GLUON Thermal Fatigue Test Package
P/N 346-99311
Applicable tests Thermal fatigue test
Applicable standard 4890 Controller
Applicable controller 4890 Controller
Recommended operating environment OS: Windows 2000, Windows XP
CPU: Pentium 800 MHz or faster
RAM: 1 GB min.
HDD: 8 GB min. free space
CD-ROM × 1 unit, 100base-T Ethernet

* Appearance and specifications are subject to change without notice.

Dynamic Characteristics Test Package

For Fundamental Evaluation of Rubber

Static Characteristics Testing Applies a constant loading rate to plot test force-displacement curves and to calculate the static spring constant.
Dynamic Characteristics Testing Applies a constant frequency or stepped frequency to calculate dynamic characteristics based on repeated cycles and the frequency.

Features

  • A constant frequency or frequency sweep test can be performed by setting dynamic characteristics. FFT or area can be selected as the characteristics value calculation method.
  • Static characteristics tests and dynamic characteristics tests can be executed continuously.
  • In data processing items, max. test force/displacement, test force of spring calculation point and static spring constant can be calculated as static characteristic values. Absolute spring constant, storage spring constant, loss spring constant, absolute complex modulus of elasticity, storage modulus of elasticity, loss modulus of elasticity, and loss sine can be calculated as dynamic characteristics values.

Specifications

Part name GLUON Dynamic Characteristics Test Package
P/N 346-99310
Applicable tests Static characteristics testing, dynamic characteristics testing
Applicable standard JIS K 6385, JIS K 6394
Applicable controller 4890 Controller
Recommended operating environment OS: Windows 2000, Windows XP
CPU: Pentium 800 MHz or faster
RAM: 1 GB min.
HDD: 8 GB min. free space
CD-ROM × 1 unit, 100base-T Ethernet

* Appearance and specifications are subject to change without notice.

Pseudo-Dynamic Test Package

For Earthquake-Response Testing of Structures

The elastic-plastic response displacement for each input seismic-wave step is taken as the target values and is controlled to reach each layer simultaneously. The Newmark β method is used for the response calculation, but user's individual response calculations can also be conducted on an external PC, for example. Vertical jacks (up to 1 layer) can be used in addition to horizontal jacks (up to 4 layers).

Features

  • Test start/end points and acceleration factor of seismic waves can be adjusted in the seismic wave settings.
  • The elastic-plastic response displacement at input of the seismic wave can be previewed when previewing this displacement.
  • Test Execution The load speed and attenuation matrix can be changed during the test.

Specifications

Part name GLUON Pseudo-Dynamic Test Package
P/N 346-99312
Applicable tests Pseudo-dynamic test
Applicable controller 4890 Controller
Recommended operating environment OS: Windows 2000, Windows XP
CPU: Pentium 800 MHz or faster
RAM: 1 GB min.
HDD: 8 GB min. free space
CD-ROM × 1 unit, 100base-T Ethernet

* Appearance and specifications are subject to change without notice.

For Research Use Only. Not for use in diagnostic procedures.

This page may contain references to products that are not available in your country. Please contact us to check the availability of these products in your country.

Top of This Page