Ceramics Bending Test Jig

Max. test force 5 kN
Applicable standards JIS R1601 (Bending Test Method for Fine Ceramics)
 
3-/4-point bending test jigs for small specimens Distance between 3-/4-point bending supports 10 to 60 mm
Span between 4-point bending punch 10 mm
3-/4-point bending test jigs for ceramics Distance between 3-/4-point bending supports 30 mm
Span between 4-point bending punch 10 mm
3-/4-point bending test jigs for composite materials Distance between 3-/4-point bending supports 30 to 100 mm
Span between 4-point bending punch 10 to 35 mm