Flexural Test Methods for Plastics: ISO 178 and JIS K 7171

ISO 178 and JIS K7171 Specimen and Fixture Dimensions
Size Recommended Specimen 3-Point Bend Test Fixture
Specimen length,l 80 mm - -
Specimen width,strong 10 mm - -
Specimen thickness,h 4 mm h> 3 mm h≦ 3 mm
Punch radius,R 1 5 mm
Support radius,R 2 5 mm 2 mm
Distance between supports,L 16h