Long-Stroke Tensile Testing System for Vulcanized Rubber

Long-Stroke Tensile Testing System

Capable of Measuring Even Specimens with a Large Break Strain

Features

A tensile test method for vulcanized rubber is stipulated in JIS K6251 (Rubber,vulcanized or thermoplastic-Determination of tensile stress-strain properties). One of the properties of vulcanized rubber is significant elongation. This long-stroke tensile testing system for vulcanized rubber has a long stroke that is required for calculating these tensile characteristics of rubber, and accommodates dumbbell specimens Nos.1 through 6 stipulated in JIS K6251.

This system is based on the Shimadzu Autograph AG Series, and consists of a "pantograph type grip" having outstanding operability, "SES-1000 Extensometer for Soft Materials" compatible with measurement of high ductility elongation, and the AG dedicated software "TRAPEZIUM2" for conducting data processing from the test force-displacement curve in real time.

This system enables you to efficiently obtain the tensile characteristics of vulcanized rubber.

Load capacity 1 kN
Grip 1 kN pantograph grip type 2
Initial grip space Dumbbell specimen No.1: 90 mm
Dumbbell specimen Nos.2, 3, 4: 70 mm
Dumbbell specimen No.5: 85 mm
Dumbbell specimen No.6: 40 mm
Tensile stroke Dumbbell specimen No.1: 655 mm
Dumbbell specimen Nos.2, 3, 4: 675 mm
Dumbbell specimen No.5: 660 mm
Dumbbell specimen No.6: 705 mm
Displacement gauge length 20, 25, 40 mm
Displacement gauge measurement range 100, 200, 1000 % at each gauge length