TGA-50/50H And TGA-51/51H

Thermogravimetric Analyzer

  • Temperature range: Room temperature to 1000°C/Room temperature to 1500°C (H-type)
  • Measurement range: ±20, ±200 mg (50-type)
  • Measurement range: ±20, ±200, ±2000 mg (51-type)
  • Maximum sample weight: 1 g (including wind bag)/10 g (including wind bag, 51-type)
 
TGA-50
TGA-50H
TGA-51
TGA-51H
Temperature Range
Ambient to
1000°C
Ambient to
1500°C
Ambient to
1000°C
Ambient to
1500°C
Weight measuring range
20mg, 200mg
20mg, 200mg, 2g
Readability
0.001mg
Sample mass
1 g including tare
10g including tare
Programmable heating rate
0.1°C/hour to 99.9°C/min
0.1°C/hour to 50.0°C/min
0.1°C/hour to 99.9°C/min
0.1°C/hour to 50.0°C/min
Hold time
0 to 999min, 0 to 999hour
Temperature program format
99 steps maximum
Temperature program file
up to 100 files
Cooling method
Air-cooled
Signal output
Analog and digital
Atmosphere control
Built-in gas flowmeter (250ml/min maximum)
Dimensions
W173xD550xH500mm
W173xD600xH540mm
Power supply
AC100V, 120V, 220V, 240V, 500VA, 50/60Hz
AC100V, 120V, 220V, 240V, 1.2kVA, 50/60Hz
AC100V, 120V, 220V, 240V, 1kVA, 50/60Hz
AC100V, 120V, 220V, 240V, 1.5kVA, 50/60Hz

For Research Use Only. Not for use in diagnostic procedures.