Flexural Test Methods for Plastics: ISO 178 and JIS K 7171
Resin materials (plastics) are found in a wide variety of items used on a daily basis. Recently, plastics have started to be used as structural materials in transportation equipment, such as automobiles and aircraft, due to their strength and light-weight nature. In these applications, it is important to understand the mechanical strength properties of these plastics.
Testing the flexural properties (bending properties) of plastics and other resin materials are covered in ISO 178 and JIS K 7171. These methods include calculations for the mechanical properties and accuracy specifications for the measuring systems used.
The ASTM standard for flexural testing of plastics, ASTM D790, has slightly different requirements compared with ISO 178 and JIS K7171, which are essentially the same. For more information about ASTM D790, please click here.

Features
-
A test force accuracy that meets ISO 7500-1 Class 1 and JIS B 7721 Class 1, accuracy within ±1% of the indicated...
-
ISO 178 and JIS K 7171 require ISO 9513 Class 1 accuracy (accuracy within 1% of the indicated value) for...
-
ncluded in the annexes of ISO 178 and JIS K 7171 are crosshead displacement and compliance correction...
-
The radius of the punch and supports of the 3-point bend test fixture used for ISO 178 and JIS K 7171 flexural test...
Applications
| Documents | Date Creation Date |
|---|---|
2019-07-15 | |
2019-02-21 | |
2018-03-29 |
News / Events
-
New Video: AUTOGRAPH AGX-V2 Voice Operation Device XV-Talk
We will introduce how XV-Talk, the world's first voice control device installed in Shimadzu's latest tensile tester AGX-V2, can be used in various scenarios.
-
New Video: AUTOGRAPH AGX-V2 Operation Control Panel Stand-alone test feature
We will introduce a new feature of Shimadzu's latest tensile tester, AGX-V2, a stand-alone testing function using a large color LCD touch panel.
-
New Autograph AGX-V2 Series Precision Universal Testing Machines
The World’s First Testing Machines Equipped with a Voice Operation Device
-
Cellulose nanofibers
Given that cellulose nanofibers(CNFs)offer attractive physical characteristics, such as light weight, strength, and hardness, they not only enable materials with advanced functionality, but are expected to be used as a reinforcing material that can reduce the weight of composite materials.
-
Latest issue of Shimadzu Journal, featuring Materials Science, has come out.
This issue focuses on Materials Science particularly on lithium-ion batteries (LiBs). It starts with two customer interviews in which users discuss their relationship with Shimadzu.
-
Hydrogen Energy Analysis Solutions for Quality Control of Hydrogen
Impurities in hydrogen production affect subsequent industrial processes. Strict purity standards have been defined for hydrogen used in fuel cells (ISO 14687-2019). This is because if hydrogen contains carbon monoxide, sulfur components, etc., the catalyst of the fuel cell will be damaged. The hydrogen fuel standard for FCVs (ISO 14687 TypeII GradeD) defines many items to be controlled, and Shimadzu analytical instruments can play a role in analyzing these items.