High accuracy quality control analysis*1 of cement is typically conducted using a wavelength dispersive X-ray fluorescence spectrometer. EDX instruments have become capable in recent years of analysis accuracy comparable to that of low-output wavelength dispersive type instruments. Not only do they offer such conveniences as the ability to analyze powders as they are, their range of applicability has greatly widened to include the analysis of such substances as cement. Here, we introduce the analysis accuracy obtained with pressure-formed cement standard powder samples using the new model EDX-8000.

Content Type:
Application
Document Number:
LAAN-A-XR-E028A
Product Type:
Elemental Analysis, Energy Dispersive X-ray Fluorescence Spectroscopy
Keywords:
EDX, Cement, Powder, Pressure forming, Calibration curve, Precision, Quantitative analysis, CaO, SiO2, Al2O3, Fe2O3, MgO, SO3, K2O, Na2O, X254, Ceramics, Metals, Mining, Glass, Cement, Ceramics, Other inorganic material, EDX-8000
Language:
English
File Name:
jpq213010.pdf
File Size:
185kb

View Article

For Research Use Only. Not for use in diagnostic procedures.

This page may contain references to products that are not available in your country. Please contact us to check the availability of these products in your country.

Top of This Page