Analysis of Brominated Flame Retardants and Phthalate Esters In Ploymers Under the Same Conditions Using a Pyrolysis GC-MS System (2) - Phthalate Esters -
This Application Data Sheet shows the results from analyzing seven phthalate esters in polymers under the same analytical conditions as those in Application Data Sheet 47 using EGA/PY-3030D Multi-Shot Pyrolyzer and GCMS-QP2020 Ultra systems.
- Content Type:
- Application
- Document Number:
- LAAN-J-MS-E048
- Product Type:
- Mass Spectrometry, Gas Chromatograph-Mass Spectrometry
- Keywords:
- PPBs, PBDEs, RoHS, FASST, BDEs, PBBs, DIBP, DBP, BBP, DEHP, REACH SVHC, DOP,DINP, Electronics, Electronic, Automotive, Environment, Electronics/Electronic device, Semi-conductor, Electronic parts, Mounting board, Printed Circuit Board, EGA/PY-3030D Multi-Shot Pyrolyzer, GCMS-QP2010 Ultra
- Language:
- English
- File Name:
- jpo112100.pdf
- File Size:
- 152kb