Determination of Chloride and Sulfate in Fuel Ethanol by Ion Chromatography
ASTM D4806-08a (American Society for Testing andMaterials (United States)) is a standard that regulates ethanol fuel, and ASTM D7319-07 specifies that ionchromatography is to be used as the official method for analyzing chlorides and sulfates in ethanol fuel. Here we present an example of analysis using the Prominence HIC-SP suppressor-type ion chromatograph which pertains only to this analytical method.
- Content Type:
- Application
- Document Number:
- L384
- Product Type:
- Liquid Chromatography
- Keywords:
- Hydrocarbon Processing Industry (Petrochemical, Chemical), Bio Fuels, Prominence, HIC-SP
- Language:
- English
- File Name:
- l384e.pdf
- File Size:
- 304kb