Analysis of Oiliness Agent Adsorption Film Formed on Surface of Iron Oxide in Lubricant by SPM-8100FM
By using the SPM-8100FM, it was possible to evaluate a comparatively hard adsorption film that formed on an iron oxide surface in a lubricant from changes in surface shape, and a flexible adsorption layer, which cannot be captured as shape change, by crosssectional imaging.