Evaluation of Dispersibility of Individualized Cellulose Nanofiber (CNF)
High-transparency monodisperse CNF and cloudy networked CNF were compared, and their transparency and dispersibility were evaluated using an ultraviolet-visible light (UV-VIS) spectrophotometer. Transparency differs and is affected by dispersibility, depending on the type of CNF.