Features
- Compact
Ideal for laboratory use, furnace is easily installed in a small space and provides same basic performance and functionality of a production model. - Designed According to Processing Requirements
Choose from graphite, molybdenum or tungsten for heater and heat-insulating layer materials.
Applications
- Various Research and Laboratory Applications
Superhard Sintering
MIM
Ceramics
Magnetic Materials
Heat Treatment
VHL/PHL Series Specifications
| Laboratory Furnace | |||||||
|---|---|---|---|---|---|---|---|
| Model | VHLgr 20/20 |
VHLgr 20/20/30 |
VHLmo 20/20/20 |
PHSgr 20/20/40 |
|||
| Effective Intern. Dim. (mm) W x H x D |
φ200×200H | 200W×200H×300L | 200W×200H×200L | 200w×200H×400L | |||
| Heater Material | Molybdenum | Graphite | |||||
| Max. Temp. (°C) | 1600 | 2200 | |||||
| Process. Cap. (kg gross) | 10 | 10 | 10 | 50 | |||
| Ultimate Press. (Pa) | 7×10-4 | ||||||
| Max. Pressure | 0.9MPa・G | ||||||
| Power Req. (kVA) | 30 | 35 | 35 | 150 | |||