EDX-8100
X-Ray Analysis
Ceramics are used in a wide range of fields. Their production process depends on raw materials, intermediate and final products. Manufacturer analyzes the chemical composition of their materials and products on each process for quality control. Component of these materials are almost inorganics, such as mineral and oxides, which can be analyzed by chemical or wet methods like gravimetric method, ICP- AES, ICP-MS, and AAS. Also, these analyses can be substituted by EDXRF; Energy Dispersive X-ray fluorescence analysis.
February 21, 2019 GMT