EHF-L Series
- Dynamic fatigue tests of endosseous dental implants conforming to ISO 14801 : 2016 and JIS T 6005 : 2020 can be conducted. - High-accuracy dynamic control is possible by using the Servo Controller 4830.
Endosseous dental implants consist of a tooth root part (implant body), an abutment which is attached to the implant body, and an artificial tooth, and are implanted in the bone of the jaw where a tooth has been lost. A titanium screw is generally used in the implant body. Although a fatigue test method for endosseous dental implants is provided in JIS T 6005 : 2020, this is not related to the fatigue characteristics of the component materials of endosseous dental implants, but rather, describes effective methods for comparing implants with various designs or dimensions. This article introduces an example of a test using a tensile test jig conforming to JIS T 6005 : 2020.
January 14, 2024 GMT
Some products may be updated to newer models