0

-Quick determination of measurement positions-​

Loading Samples Is Easy

Load Sample

Pressing the [Eject Sample] button makes it easy to load and remove samples by automatically lowering the stage and switching the objectives to expand space. Furthermore, the lower Condenser mirror can be removed to enable reflectance/ATR measurements of samples up to 40 mm thick.



 

Look for the Item to be Measured
-Quickly Determine the Measurement Position-

Wide-Field Camera and Microscope Camera

Look for the Item to be Measured

Golden object on a metal plate

The wide-field camera and microscope camera help observe samples efficiently. In addition to observing a large area up to 10 × 13 mm, the wide-field camera also supports variable digital zooming. Furthermore, by sharing positional information with the microscope camera, it achieves a digital zoom function capable of zooming to a magnification of about 330× for observing areas as small as 30 × 40 µm. (The microscope camera supports variable digital zoom magnifications up to 10×.)

Perform Infrared Measurements Smoothly While Viewing Visible Images
- Visible/Infrared Dual View System -

Dual View System

Infrared spectra can be measured while checking a visible image of the sample. Spectra can be measured while confirming the position of objects, which avoids the trouble of switching back and forth between visible light and infrared light. Used in combination with the tiling function, visible observations, and infrared measurements can be performed anywhere within the stage operating range, eliminating the need to reposition the sample.

Image view of the visible light and infrared optical path
          Green light: visible light optical path
          Red light : infrared optical path         

-Automatic recognition of targets-​

Automatic Contaminant Recognition System

 ANALYTICAL INTELLIGENCE

  • The functionality for automatically recognizing objects is included standard. The analyst simply clicks one button for the software to automatically recognize objects. Two types are available: the standard type or the micro type for extremely small areas, which can be selected based on the purpose of analysis. Samples can either be measured with the automatically selected measurement positions left unchanged or the analyst can add or delete measurement positions. A sample image is automatically saved for each measured spectrum. That makes it easy to confirm the sample or measurement positions later.
  • Automatic Contaminant Recognition System

 

Perform Ultra Micro Analysis  - Best-in-Class S/N Ratio-

The AIMsight has been optimized to measure extremely small areas. The AIMsight achieves a 30,000:1 S/N ratio, the best in its class. Consequently, it can quickly obtain excellent spectra from even microscopic objects.

 

 

Transmission measurement of polystyrene beads

A ø10 μm polystyrene bead was measured by transmission method. Low noise and a high-quality spectrum of a very small sample were obtained with only a small number of scans.

Perform Ultra Micro Analysis

 

 

High-Sensitivity ATR Measurement  - Samples with High Refractive Index -

Due to a steep incident angle for the infrared light, the AIMsight is able to acquire excellent distortion-free ATR spectra even when measuring samples with a high refractive index, such as black rubber. In addition, the Ge prism (P/N 206-32600-41) has an anti-reflective coating that provides high sensitivity.

ATR measurement of black rubber
An acrylonitrilebutadiene rubber (NBR) with 50 wt% carbon was measured with a 
Ge-ATR objective. A clear peak of C=C-H out-of-plane bending mode was obtained at 970 cm-1, which was strained with a gradual incident angle.                                                   

High-sensitivity ATR measurements

 

Length Measurement Function

A length measurement function has been added to AMsolution. The length of the target object can now be measured in images obtained with the infrared microscope.
In addition, with a single click, the length measurement results can be output as a report.

Length Measurement Function

 

-Automatic identification of objects-​

Fully Supports the Identification of Contaminants

Various libraries are available, such as Contaminant Library, Thermally-Damaged and UV-Damaged Plastic Library.

Automatic Identification of Object
-Contaminant Analysis Program-

ANALYTICAL INTELLIGENCE

The contaminant analysis program - the functionality for automatically qualifying objects - is included as a standard feature in LabSolutions™ IR software. Measured spectra using AMsolution can be loaded directly into LabSolutions IR and analyzed. The contaminant analysis program identifies measured objects with high precision using a spectral library for substances commonly detected as contaminants in combination with Shimadzu's proprietary identification algorithm (patent JP5205918). Even if objects are mixtures, the system searches for the primary and secondary components and displays the probability of the substances identified. It is not necessary to specify the number of components in the mixture, so analysis is easy, even for people with little experience with infrared analysis.

Spectrum Advisor Function (patent pending)

ANALYTICAL INTELLIGENCE
 

This is packaged with operations specific to infrared microscopes and advice on troubleshooting using accessories. Corrective measures are proposed by comparing the measured spectrum with measurement examples. As a result, better-quality data can be acquired.

Spectrum Adviser
 

Visualize Components  - Chemical Imaging* -

The invisible distribution of chemicals can be visualized based on peak height or area, multivariate analysis (PCR/MCR), or spectral similarity to target spectra.

Chemical image of pharmaceutical powder

Pharmaceutical products were rolled with a diamond cell, then mapping measurement was performed. The figure to the right represents the distribution of powder components, such as lactose, lipid, and cellulose. The color display can be switched freely between single-color and multi-color.
 

Chemical image of a pharmaceutical powder

* Visualizing chemicals requires an optional high-speed mapping program (P/N 206-36299-41).

 