Language
Español
English
0

SSG10-10

Measurement range (mm/FS)

1.0,0.5,0.2,0.1
Four-step
selection

Gauge length (mm)

10

Max. measurement range (mm)

1

Max. specimen size (mm) : Rod maximum diameter

φ10

Max. specimen size (mm) : Flat plate width x thickness

W15×T10

Accuracy

JIS Class 1 ASTM Class CMeasurement range up to 0.3 mm: ± 3 μmMeasurement range above 0.3 mm to max.: ±1.0% of indicated value

Operational temp. range

5 to 40°C (JIS guaranteed precision range: Fluctuation within ±2°C at 18 to 28°C)

Power Requirements

ESA type amplifier: Single-phase 100 V to 240 V AC at 150 VA
(SGX type amplifier requires no power supply.)

Read more
Show Less

SSG25-10

Measurement range (mm/FS)

2.5,1.25,0.5,0.25
Four-step
selection

Gauge length (mm)

25

Max. measurement range (mm)

2.5

Max. specimen size (mm) : Rod maximum diameter

φ10

Max. specimen size (mm) : Flat plate width x thickness

W15×T10

Accuracy

JIS Class 1 ASTM Class CMeasurement range up to 0.3 mm: ± 3 μmMeasurement range above 0.3 mm to max.: ±1.0% of indicated value

Operational temp. range

5 to 40°C (JIS guaranteed precision range: Fluctuation within ±2°C at 18 to 28°C)

Power Requirements

ESA type amplifier: Single-phase 100 V to 240 V AC at 150 VA
(SGX type amplifier requires no power supply.)

Read more
Show Less

SSG50-10

Measurement range (mm/FS)

5,2.5,1.0,0.5
Four-step
selection

Gauge length (mm)

50

Max. measurement range (mm)

5

Max. specimen size (mm) : Rod maximum diameter

φ15

Max. specimen size (mm) : Flat plate width x thickness

W25×T14

Accuracy

Measurement range 0 to 0.13 mm: ±1 μmMeasurement range 0.13 mm to 0.3 mm: ±3 μmMeasurement range 0.3 mm to 5 mm: ±1.0% of indicated value

Operational temp. range

5 to 40°C (JIS guaranteed precision range: Fluctuation within ±2°C at 18 to 28°C)

Weight

about 75g

Power Requirements

ESA type amplifier: Single-phase 100 V to 240 V AC at 150 VA
(SGX type amplifier requires no power supply.)

Read more
Show Less