EDXIR-Analysis Contaminant Finder/Material Inspector - Specs
EDX-FTIR Contaminant Finder/Material Inspector
Example of the Data Contained in a Library
| Name | Comment | |
| Water Supply Related Contaminants | Pipe slip packing |
Materials; Polyethylene (PE), |
| Sealing tape |
Materials; Polytetrafluoroethylene (PTFE), |
|
| Coating of inner wall_1 |
Materials; Polystyrene (PS), Acrylic resin, |
|
| Mold |
Materials; Protein, Silicate, |
|
| Coating in pump_white |
Materials; Polyamide (Nylon11), Titanium dioxide (TiO2), |
|
| Food Related Contaminants |
Piece of plant material |
Materials; Plant epidermis (Cellulose), Vegetable fat (Triacylglycerol), |
| White hair |
Materials; Human hair (Protein), |
|
| Nail |
Materials; Nail (Keratin), |
|
| Bone particle_brown |
Materials; Bone particle (Calcium phosphate, Protein), |
|
| Staplor1 |
Materials; Zinc stearate (Surface contaminant), |
|
| Glass fragment |
Materials; Glass (SiO2), |
|
| Stainless steel_1 |
Materials; Metal Metal, |
|
Main Specifications
EDXIR-Analysis Software
| Item | Conditions |
| Applicable Models | EDX: EDX-7000/8000 FTIR: Instruments that can be controlled by LabSolutions IR/IRsolution/AIMsolution |
| Operating System (OS) | Windows® 10 Pro 64-bit Windows® 11 Pro |
| Profiles and Spectral Data Files That Can Be Loaded | EDX profiles (*.datqlqn) LabSolutions IR data files (*.ispd) IRsolution data files (*.smf) AIMsolution data files (*.apit) JCAMP data files (*.DX, *.JDX) |
| Other Files That Can Be Loaded | Bitmap files (*.bmp) PNG files (*.png) JPEG files (*.jpg) PDF files (*.pdf) |
| Number of Libraries That Can Be Created | Up to 100 libraries |
| Number of Libraries That Can Be Used in Searches | Up to 64 libraries |
| Number of Data That Can Be Registered in a Library | Up to 2,000 data |
Downloads
Download the latest brochure.