Ferroelectric (TGS) Cleavage Surface (3)

Observation Conditions: Temperature: 22 to 23 °C; Humidity: 55 to 65 %

Observations were made of changes over time to the half lattice step pattern of the cleavage surface of TGS (ferroelectric tri-glycine sulfate). The pattern changes were likely caused by surface diffusion of ions released from the steps.
(Data provided by: Associate Prof. Makoto Iwata, Graduate School of Engineering, Nagoya Institute of Technology)