Analysis of Plastic
Download
Introduction
An ICP emission spectrometer can be used to accurately measure low concentrations of harmful metals like lead and cadmium in plastics. Decomposition of plastic samples for analysis is conducted by the dry-ashing, wet decomposition or microwave digestion method. This application introduces the analysis of plastic using the multi-type ICPE-9000 ICP emission spectrometer.
September 24, 2009 GMT