CFRP Quality Control - CFRP and GFRP Orientation Analysis -
CFRP and GFRP Orientation Analysis
Analysis and Observation of the Internal Structure of CFRP and GFRP via a Microfocus X-Ray CT System
Combining a variety of fibers to increase product strength is standard practice. Detailed observation and analysis of the flow of these fibers is important as they have a significant impact on a product's strength.
The Microfocus X-Ray CT System can make 3-dimensional observations of the orientation of fibers, and can perform non-destructive observations of fiber coarseness and fineness, resin bubbles (voids), and cracks.
Example of CFRP Observation
![](/an/sites/shimadzu.com.an/files/d7/ckeditor/an/industry/ceramicsmetalsmining/cfrp/n9j25k0000056x6l-img/n9j25k0000056x9h.jpg)
The fibers are carbon, and the black spots are air bubbles (voids).
The parts (welds) where the flow of the fibers has changed can be observed.
Example of GFRP Analysis
![](/an/sites/shimadzu.com.an/files/d7/ckeditor/an/industry/ceramicsmetalsmining/cfrp/n9j25k0000056x6l-img/n9j25k0000056xa0.jpg)
By extracting only the fibers and thinning them, it is possible to measure the fiber orientation, density, and number of intersections.
Samples provided by: Yokoi Lab., Institute of Industrial Science, the University of Tokyo