JIS K6911 / JIS K6902 / JIS C6481 / JIS K7171, etc.
Applicable standards
Load capacity
10 kN
Distance between supports
20 to 200 mm
Temperature range
0 to 40 °C
ASTM D790
Applicable standards
Load capacity
10 kN
Distance between supports
0.8 to 8''
Temperature range
0 to 40 °C
JIS K6911 / JIS K6902 / JIS C6481 / JIS K7171, etc.
Applicable standards
Load capacity
100 kN
Distance between supports
50 to 500 mm
Temperature range
0 to 40 °C
ASTM D790
Applicable standards
Load capacity
100 kN
Distance between supports
2 to 20''
Temperature range
0 to 40 °C