Glossy Inkjet Paper

The silica powder used in the uppermost coating of the paper can be seen in the topographic image (left). The phase image (right) shows particles from several nanometers to tens of nanometers even more clearly.

The silica powder used in the uppermost coating of the paper can be seen in the topographic image (left). The phase image (right) shows particles from several nanometers to tens of nanometers even more clearly.