40Next-Generation Mobility Technology Evaluation C10G-E098A Next-Generation Mobility Technology Evaluation www.shimadzu.com/an/ For Research Use Only. Not for use in diagnostic procedures. This publication may contain references to products that are n ...
15 de ene. de 2026
User Benefits Application News 50 µm COMPO 15.0 kV 200× 150 µm 10 µm 10 µm Mg Ka 15.0 kV × 3000 4.80 (wt%) 0.00 4.20 3.60 3.00 2.40 1.80 1.20 0.60 10 µm Al Ka 15.0 kV × 3000 3.20 (wt%) 0.00 2.80 2.40 2.00 1.60 1.20 0.80 0.40 10 µm Fe Ka 15.0 kV × 30 ...
25 de nov. de 2025
User Benefits Application News Fig. 1 Representation of E-PBF 3D Printing process The size and shape of the specimens is shown in Fig.2. Firstly,a cylindrical sample with a radius of 10mm was created with theelectron beam PBF technique, and then mac ...
26 de dic. de 2023
User Benefits Application News Analysis of Fe-Al Bonded Dissimilar Materials by EPMA and X-Ray CT X-ray CT (computed tomography) is useful in research such as study of welding conditions, as changes in composition and internal microstructure can b ...
28 de jun. de 2022
User Benefits Application News Fig. 1 Mapping of Power Semiconductor Power semiconductors are used in a wide range of applications, from household electrical appliances and automotive devices to power transmission and distribution systems. Recently, ...
17 de sep. de 2025
User Benefits Application News Fig. 1 External Appearance of Sintered Ore after Reduction Fig. 3 Mapping of Sintered Ore after 600 ˚C Reduction Reduction of carbon dioxide (CO 2 ) emissions is being promoted with the aim of achieving carbon neutrali ...
12 de mar. de 2025
User Benefits Application News (basicity) 10 µm Al Ka 15.0 kV × 3000 2.40 (wt%) 0.00 2.10 1.80 1.50 1.20 0.90 0.60 0.30 10 µm Mg Ka 15.0 kV × 3000 1.44 (wt%) 0.00 1.26 1.08 0.90 0.72 0.54 0.36 0.18 10 µm COMPO 15.0 kV × 3000 10 µm Fe Ka 15.0 kV × 30 ...
20 de feb. de 2024
User Benefits Application News Sintered ore consists of hematite, magnetite, calcium ferrite, and slag. The OM-image in Fig. 1 is an optical microscope image of sintered ore, in which hematite (Fe 2 O 3 ) is observed as a high- brightness structure ...
12 de sep. de 2023
Application News No. P112 EPMA-8050G Electron Probe Microanalyzer Analysis of Automotive Three-Way Catalyst In modern society, environmental countermeasures have evolved with the progress of motorization together with high economic growth. Automot ...
1 de ago. de 2020
Application News No. P114 EPMA-8050G Electron Probe Microanalyzer Analysis of Inorganic Antimicrobial Agents Introduction In response to a heightened awareness of cleanliness, antimicrobial treatment has been applied not only to processed goods ...
27 de oct. de 2020
Most of the documents on the LITERATURE is available in PDF format. You will need Adobe Acrobat Reader to open and read PDF documents. If you do not already have Acrobat Reader, you can download it free at the Adobe's Website. Click the GET ADOBE READER icon on the left to download a free copy of Adobe Acrobat Reader.