Surface Analysis of PET Film Using a Benchtop MALDI-TOF Mass Spectrometer

MALDI-TOF Mass Spectrometry

Download

Introduction

MALDI-TOF mass spectrometers are a mass spectrometer type that is used in a wide range of fields likewise LCMS, in terms of high through-put and high sensitivity. These instruments have recently being utilized more and more for simple molecular weight measurement and profiling of synthesized products and high-molecular compounds. This is because instruments of this type have several features: singly-charged ions are generated so molecular weights can be recognized easily, the mass range is wide, and there are many solvent options because the sample is dried before measurement. On the other hand, due to changes in social conditions in these several years, government offices, universities, and private enterprises strongly request the reduction of costs for both introduction and running of instruments used for such applications. The benchtop "MALDI-8020" MALDI-TOF mass spectrometer is a new instrument that can sufficiently meet such market needs. The noteworthy point of this instrument is that it has a shorter flight tube, which is the key feature of its small size, while retaining the performance equal to or higher than that of a conventional model. In recent years, the usability of MS imaging using a MALDI-TOF mass spectrometer has become widely recognized and various techniques are being developed. On the other hand, needs for examining the compounds that exist on surfaces, rather than its "microscopic structure", are increasing in association with degradation and durability tests. This article introduces an example of analyzing a PET film surface using the benchtop MALDI-TOF mass spectrometer "MALDI-8020".

November 6, 2017 GMT

Related Products

Some products may be updated to newer models