Observations of a Resin Cable Clamp Using the inspeXio SMX-90CT Plus Benchtop Micro Focus X-Ray CT System

Download

Introduction

Industrial X-ray CT systems have been widely used for inspections and structural analyses of a variety of products including electronic parts, automobile parts, and resin molded products. More recently, such systems have also proven useful for observing the internal structure and form of resin molded products. In Application News No. N119, we introduced an example of the measurement of a resin connector using the inspeXio SMX-100CT. Here, we introduce an example of the observation and analysis of a resin cable clamp using a newer, smaller benchtop X-ray CT system.

November 26, 2014 GMT