Most of the documents on the LITERATURE is available in PDF format. You will need Adobe Acrobat Reader to open and read PDF documents. If you do not already have Acrobat Reader, you can download it free at the Adobe's Website. Click the GET ADOBE READER icon on the left to download a free copy of Adobe Acrobat Reader.

High-Speed Tensile Test Measurement Data

Data example for plastics

Material : Polycarbonate
Flat plate : 5 mm wide x 2 mm thick
Tensile rate : 20 m/s

Data example for aluminum

Round rod : 5 mm radius
Tensile rate : 5 m/s

Puncture Impact Measurement Data

Data example for plastics

Material : Polycarbonate (t = 2 mm)
Speed : 10 m/s

Data example for aluminum

Material : Aluminum (t = 0.75 mm)
Speed : 20 m/s