- Use of the Microservo MMT series of magnetic micro testing system enables evaluation of the fatigue and durability of small specimens. - High-accuracy dynamic control can be achieved by using the Servo Controller 4830.

Introduction

Fatigue tests are tests to evaluate the fatigue life of materials, in which cyclical loading is applied repeatedly to the material. Considering the risk of a serious accident if fatigue fracture occurs, fatigue tests are indispensable for developing highly reliable products. This article introduces a fatigue test of a small aluminum alloy test specimen using an MMT-250NV-10 Microservo magnetic micro testing system. The MMT series has the advantages of high-speed, high-accuracy control of small test forces and displacement, and is suitable for fatigue testing of small test specimens.