FTIR accessory selection guide

In order to make full use of the impressive functionality offered by FTIR spectrophotometers, the optimal accessories must be selected based on the given application field or sample characteristics.
Select the attachments and accessories best suited to given analytical objectives using Shimadzu FTIR series spectrophotometers.
There are many other accessories available that are not featured here. Please let us know your requirements.
| Sample | Analytical form and analytical condition | Accessory | ||
|---|---|---|---|---|
| Solids | Rubbers | Total reflectance method | Multi-bound ATR such as ATR-8000A, ATR-8200HA, HATR10 | |
| Single-bound ATR such as QATR series, MIRacle series, Quest, MicromATR series | ||||
| Liquid film method | Demountable cell | |||
| Powders | Total reflectance method | Multi-bound ATR such as ATR-8000A, ATR-8200HA, HATR10 | ||
| Single-bound ATR such as QATR series, MIRacle series, Quest, MicromATR series | ||||
| KBr pellet method | KBr die + hydraulic press + vacuum pump | |||
| Nujol method | Demountable cell | |||
| Diffuse reflectance method | DRS-8000A(mix with KBr powder) | |||
| Paper, cloth, yarns | Total reflectance method | Multi-bound ATR such as ATR-8000A, ATR-8200HA, HATR10 | ||
| Single-bound ATR such as QATR series, MIRacle series, Quest, MicromATR series | ||||
| Transmission method | Film holder (Use a grid polarizer for study of molecular orientation) | |||
| Film, plastics | Total reflectance method | Multi-bound ATR such as ATR-8000A, ATR-8200HA, HATR10 | ||
| Single-bound ATR such as QATR series, MIRacle series, Quest, MicromATR series | ||||
| Transmission method | Film holder (Use a grid polarizer for study of molecular orientation) | |||
| Film method | Demountable cell (Evaporate the solvent to obtain the film) | |||
| Grind | SiC sampler | |||
| Coating films on metals | Thicker than 1µm | Total reflectance method | Multi-bound ATR such as ATR-8000A, ATR-8200HA, HATR10 | |
| Single-bound ATR such as QATR series, MIRacle series, Quest, MicromATR series | ||||
| Measurement to a depth of 1/5 of the wavelength with a Diamond, ZnSe or KRS-5 prism and to 1/10 with a Ge prism | ||||
| Specular reflectance method | SRM-8000A | |||
| Thinner than 1µm | Reflection absorption spectrometry | RAS-8000A (Use of a grid polarizer enhances sensitivity about two times) | ||
| Diffuse reflectance method | DRS-8000A | |||
| Coating films on resins | Total reflectance method | Multi-bound ATR such as ATR-8000A, ATR-8200HA, HATR10 | ||
| Single-bound ATR such as QATR series, MIRacle series, Quest, MicromATR series | ||||
| Measurement to a depth of 1/5 of the wavelength with a Diamond, ZnSe or KRS-5 prism and to 1/10 with a Ge prism | ||||
| Specular reflectance method | SRM-8000A (Convert a reflection spectrum into an absorption spectrum by the Kramers-Kronig method) | |||
| Semiconductors | Direct measurement | Film holder | ||
| Liquids | Oil content measurement | Measures mineral oils only | Quartz cell | |
| Also measures animal/plant oils | CaF2 cell | |||
| Nonvolatile organic solvents | Liquid film method | Demountable cell | ||
| Total reflectance method | Multi-bound ATR such as ATR-8000A, ATR-8200HA, HATR10 | |||
| Single-bound ATR such as QATR series, MIRacle series, Quest, MicromATR series | ||||
| Volatile organic solvents | Solution method | Fixed thickness cell, sealed liquid cell | ||
| Rapid measurement | Liquid film method | Demountable cell | ||
| Total reflectance method | Multi-bound ATR such as ATR-8000A, ATR-8200HA, HATR10 | |||
| Single-bound ATR such as QATR series, MIRacle series, Quest, MicromATR series | ||||
| Aqueous solutions | Above 10% in concentration | Liquid film method | Demountable cell with KRS-5 | |
| Below 10% in concentration | ATR method | Horizontal type or cylinder internal reflection type ATR attachment | ||
| Total reflectance method | Multi-bound ATR such as ATR-8000A, ATR-8200HA, HATR10 | |||
| Single-bound ATR such as QATR series, MIRacle series, Quest, MicromATR series | ||||
| Extract solutions | Difference spectrometry | Solution method | Fixed thickness cell | |
| Evaporate solvent | Diffuse reflectance method | DRS-8000A(The sample solution is supplied dropwise on KBr powder and measured after evaporating the solvent) | ||
| Total reflectance method | Multi-bound ATR such as ATR-8000A, ATR-8200HA, HATR10 | |||
| Single-bound ATR such as QATR series, MIRacle series, Quest, MicromATR series | ||||
| Gases | % level | 5 cm/10 cm gas cell | ||
| ppm level | Long-path gas cell(Detection limit is 0.1 to 1 ppm with 10 m optical path) | |||
| Micro/trace samples | Liquids(µL level) | Micro cell | ||
| Solids(µm level) | AIMsight (Applicable to transmission, reflection, and ATR methods) | |||
News / Events
-
Shimadzu IR 70th Anniversary
This year we celebrate 70 years of Shimadzu IR.
We launched our double-beam recording infrared spectrophotometer in 1956.In 1984, we introduced our first Fourier transform infrared (FTIR) spectrophotometer,
and in 2017, we launched a compact, high-performance FTIR system.
We will continue to evolve proactively,responding to our customers’ analytical challenges and expectations and helping to solve current and future societal issues. -
Particle Analysis System for Microplastics has been released
This system can quickly calculate the number of particles, area, volume, mass, and individual particle qualities of microplastics based on the measurement results from an infrared microscope or an infrared Raman microscope.
-
UV-Vis Spectrophotometer UV-2600i Plus/UV-2700i Plus has been released
Accommodating a wide range of accessories, UV-2600i Plus/UV-2700i Plus excels in diverse applications, measures slight absorbance differences, and ensures robust data management and compliance.
-
UV-Vis Spectrophotometer UV-1900i Plus has been released
Experience unmatched precision and ease with UV-1900i Plus. Featuring a refined user-friendly interface, ultra high-speed scanning, and comprehensive support functions, UV-1900i Plus ensures accurate and efficient measurements for all your needs.
-
TEC MCT (Peltier Cooled MCT) Detector is now available
Equipping the AIMsight Infrared Microscope or the AIRsight Infrared/Raman Microscope with the TEC MCT (peltier cooled MCT) detector makes it possible to obtain infrared spectra without using liquid nitrogen.
-
FTIR TALK LETTER Vol. 43 has been published
The article about the Introduction to the Spectrum Advisor can be used on all Shimadzu FTIR systems controlled by LabSolutions IR. Learn the key points of infrared spectral analysis for aliphatic unsaturated hydrocarbons and aromatics.